Specification: Tensile strength-(ksi)Mpa:(70)480 Yield strength at 0.2% offset-(ksi)Mpa:(58)400 Elongation(%):22min. Hardness -(HV)HRC:(-)- Preheat and Interpass:- PWHT:- IV-40°C(J):103 Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.04 Si:0.28 Mn:1.44 P:0.019 S:0.009 Cr:0.01 Ni:0.01 Mo:0.01 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.35 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/