Specification: Tensile strength-(ksi)Mpa:(100)690 Yield strength at 0.2% offset-(ksi)Mpa:(88)610 Elongation(%):16min. Hardness -(HV)HRC:(-)- Preheat and Interpass:350°F~450°F(180°C~230°C) PWHT:1380°F±25°F(750°±15°C) in 2 Hour IV0°C(J):68 Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.12 Si:0.6 Mn:2 P:- S:- Cr:10.5 Ni:0.01 Mo:1.2 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.15 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/